BHS tile line C car tile paper 80 Cree paper 90 grams when the production of the whole door width longitudinal blistering is what causes

BHS tile line C car tile paper 80 Cree paper 90 grams when the production of the whole door width longitudinal blistering is what causes

One: wave wheel pressure is a little smaller, the brake is smaller, try, I hope it can help you.

Two: tile stick pressure. Tile paper force. Speed should be adjusted, see the picture of corrugated molding is not good

Three: the paste wheel and tile stick to test the round beating! Is the gap between the paste wheel and the stick too large? Low-weight gap should also be very small! 10 silk about this 80 grams of paper

Four: It is recommended to check the paste wheel, scraping stick bearings and remove the impurities adhering to the surface of the corrugated stick.

5: Adjust the width of the glue to be 1mm smaller than the width of the paper. If the glue is too wide and the raw material is too low, the paper will be full of sons and gums, which will simply stick to the corrugated stick and form irregular fluting.

Six: The gap between the paste wheel and the pit roller is a bit large.